    I'm just happy,,,,want to share this with you. Hope i'm patient until this arrives .



    I present to you.. Mr reynolds (not burt).Horn scales,, 7/8.. what should i do about the water spots??
    Attached Images Attached Images   

  2. #2
    Know thyself holli4pirating's Avatar
    Join Date
    Feb 2008
    Location
    Rochester, New York
    Posts
    10,480
    Thanks
    122
    Thanked 2,295 Times in 1,545 Posts

    Default

    Try some Maas, but I have a feeling she'd need sanding to get those stains out. I hope that pitting by the edge isn't problematic, but I fear it will be...

  3. #3
    Still Stone Crazy After All :-( JimmyHAD's Avatar
    Join Date
    Feb 2008
    Posts
    18,097
    Thanks
    2,125
    Thanked 6,733 Times in 4,070 Posts

    Default

    When you get it try setting the bevel and see if the pitting is going to give you a swiss cheese edge before you invest a lot of time in sanding the spots. If it was mine, once I found the pitting at the bevel didn't go far and I could get to good steel, I would just Semichrome it with a paper towel and live with the spots.

  4. #4
    Senior Member ri7ani's Avatar
    Join Date
    Sep 2009
    Location
    montreal , canada
    Posts
    195
    Thanks
    84
    Thanked 29 Times in 27 Posts

    Default BUT

    the seller confirms it to be water spots and not rust

  5. #5
    Still Stone Crazy After All :-( JimmyHAD's Avatar
    Join Date
    Feb 2008
    Posts
    18,097
    Thanks
    2,125
    Thanked 6,733 Times in 4,070 Posts

    Default

    Quote Originally Posted by ri7ani View Post
    the seller confirms it to be water spots and not rust
    Cool try the Maas or whatever metal polish on a paper towel. Personally I just don't have the patience and fortitude to hand sand of hours and would rather live with a bit of patina. YMMV.

  6. The Following User Says Thank You to JimmyHAD For This Useful Post:

    ri7ani (03-12-2010)

  7. #6
    Senior Member ri7ani's Avatar
    Join Date
    Sep 2009
    Location
    montreal , canada
    Posts
    195
    Thanks
    84
    Thanked 29 Times in 27 Posts

    Default uhum!!!

    Semichrome it with a paper towel??????? you mean polishing???

  8. #7
    no class stimpy52's Avatar
    Join Date
    Jul 2009
    Location
    Irondequoit, NY
    Posts
    805
    Thanks
    76
    Thanked 153 Times in 112 Posts

    Default down the middle of the road

    Semichrome, Maas, Flitz... if the spots are a little stubborn, try just a dab of one of these polishes with a little piece of #2500 wet/dry sandpaper. It will give you a good idea where you stand without much time, effort, or destruction.

  9. The Following User Says Thank You to stimpy52 For This Useful Post:

    ri7ani (03-15-2010)

  10. #8
    Know thyself holli4pirating's Avatar
    Join Date
    Feb 2008
    Location
    Rochester, New York
    Posts
    10,480
    Thanks
    122
    Thanked 2,295 Times in 1,545 Posts

    Default

    Quote Originally Posted by ri7ani View Post
    the seller confirms it to be water spots and not rust
    If you define rust as red stuff, no, clearly there is none. But clearly there is staining and pitting. Pitting is where corrosion ate away at the metal; it can usually be found under rust. Perhaps there was once rust on that blade, or perhaps something else caused the pitting.

    Rust, if it is present, is easy to get rid of; it can be scraped right off or removed with some metal polish. It's the pitting underneath that is the real problem.

  11. The Following User Says Thank You to holli4pirating For This Useful Post:

    ri7ani (03-15-2010)

  12. #9
    no class stimpy52's Avatar
    Join Date
    Jul 2009
    Location
    Irondequoit, NY
    Posts
    805
    Thanks
    76
    Thanked 153 Times in 112 Posts

    Default ripe for honing?

    Quote Originally Posted by holli4pirating View Post
    If you define rust as red stuff, no, clearly there is none. But clearly there is staining and pitting. Pitting is where corrosion ate away at the metal; it can usually be found under rust. Perhaps there was once rust on that blade, or perhaps something else caused the pitting.

    Rust, if it is present, is easy to get rid of; it can be scraped right off or removed with some metal polish. It's the pitting underneath that is the real problem.
    Dylan -- did you want to leap in and spend a few days honing that one?

  13. The Following User Says Thank You to stimpy52 For This Useful Post:

    wrl (03-21-2010)

  14. #10
    Senior Member Maskwa's Avatar
    Join Date
    Dec 2009
    Location
    Honing in Canada
    Posts
    167
    Thanks
    22
    Thanked 39 Times in 20 Posts

    Default

    Nice looking razor.

  15. The Following User Says Thank You to Maskwa For This Useful Post:

    ri7ani (03-22-2010)

Page 1 of 2 12 LastLast

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •